Metal profile NS-18 is used both internal, and external protective element of wall facing, and also as a roofing covering. In particular, pitched roofs of various kinds of buildings in the industrial and private sectors. NS-18 is also used for fencing, fencing where heavy loads are excluded, however, the price of this metal profile is acceptable.







































Corrugated sheet HC-18
All Eurobud products are made exclusively from high-quality imported raw materials
We work only with new modern European equipment
We offer a wide range of colors and 2 types of coating: glossy polyester and matte polyester
We provide our own specialized transport for the delivery of wholesale orders
- 1140mm – full width of the metal profile
- 1100mm – useful width of the metal profile

The scheme of assembly of a roofing corrugated board with a capillary groove without stiffening ribs H18
- 1140mm – full width of the metal profile
- 1100mm – useful width of the metal profile

The scheme of assembly of a wall corrugated flooring with stiffening ribs C18
- 1140mm – full width of the metal profile
- 1100mm – useful width of the metal profile

The scheme of assembly of corrugated walling without stiffeners C18
- 1140mm – full width of the metal profile
- 1100mm – useful width of the metal profile

Scheme of assembly of corrugated wall decking with stiffening ribs C18
- 1140mm – full width of the metal profile
- 1100mm – useful width of the metal profile

Scheme of assembly of corrugated wall decking without stiffeners C18 O
Specifications | |
sheet thickness | 0,4 – 0,5 mm |
sheet length | 0,1 m – 8 m |
weight 1 sq. m. | 4-5 kg |
the thickness of the polymer coating | 25 microns – glossy polyester |
35 microns – matte polyester | |
wave height | 17,5 mm |
full sheet width | 1140 mm |
Useful sheet width | 1100 mm |
application of a protective film | production with a protective film or without it is possible |
the minimum angle of inclination of a pitched roof | 14 º |
color scale | according to the RAL color chart |
The metal tile is made of hot-dip galvanized metal covered with a multilayer bilateral polymeric protective covering. Consider in more detail the production process, metal structure and types of coatings. Cold-rolled steel sheet with a high degree of ductility is galvanized by immersion in a container with boiling zinc (hot-dip galvanizing), then applied on both sides at least 3 layers: passive anti-corrosion layer, a layer of primer and polymer coating. The layer of polymer coating is the most important because it gives the metal the appropriate color and structure (on the outside, on the inside – a protective polymer coating of smaller thickness, neutral color) and in direct contact with external factors.
Consider the types of polymer coating:
Glossy polyester – a polymer coating based on polyester paint. Characteristics: resistance of color, to action of corrosion and ultraviolet radiation, approaches various climatic conditions, maintains temperature difference from -60 to + 120oC. The thickness of the coating is 25 microns, of which polyester – 20 microns, primer – 5 microns. Requires care during delivery and installation, as careless handling can cause scratches and damage to the coating. The texture of the surface with this coating is smooth and shiny.
Matte coarse-grained polyester is a type of polyester coating that is processed at a certain stage of production, during which the coating acquires a matte structure, velvety appearance, deeper color, which becomes similar to clay tiles. The coating thickness is 35 microns, it is characterized by higher resistance to mechanical damage to the surface and the influence of sunlight on the color.
Double-sided polymer coating – a coating identical to glossy polyester, in which the polymer coating is applied on both sides of a steel sheet of the same color and thickness. This feature is very important when building fences that look equally good on both sides.
It should be remembered that the service life of metal products will be as long as possible if: the product was not mechanically or chemically damaged during loading, unloading, delivery and installation; during storage and operation, the lower and upper parts of the metal must be ventilated to prevent condensation; service life is also significantly reduced if metal products come into contact with aggressive atmospheric or chemical environments (salty sea air, acid rain near large chemical plants, cement dust, bird droppings, etc.).
- Poliester glossiness:
- Poliester matte:
- Polyester gloss bilateral:
- Poliester Printech